Verified performance data across our core film ranges. All values measured in our in-house ISO-aligned laboratory.
| Property | Testing Standard | Machine Stretch (15µm) | Hand Wrap (20µm) | Stretch Hood (100µm) |
|---|---|---|---|---|
| Tensile Strength (MD) | ASTM D882 | ≥ 45 MPa | ≥ 38 MPa | ≥ 32 MPa |
| Tensile Strength (TD) | ASTM D882 | ≥ 35 MPa | ≥ 30 MPa | ≥ 30 MPa |
| Elongation at Break (MD) | ASTM D882 | ≥ 500% | ≥ 450% | ≥ 650% |
| Elongation at Break (TD) | ASTM D882 | ≥ 650% | ≥ 600% | ≥ 700% |
| Dart Drop Impact | ASTM D1709 | ≥ 180 g | ≥ 140 g | ≥ 450 g |
| Pre-Stretch Capability | Factory Test | Up to 300% | N/A (Manual) | ≥ 85% Elastic Recovery |
| Recommended Pallet | AS 4068 | 1165 × 1165 mm | 1165 × 1165 mm | 1165 × 1165 mm |